解决方案
 
Prismatic Cell: Negative electrode tab welding appearance defect detection


    Project description: 


      This project is located after the cell winding/stacking, involving the inspection of the electrode tab welding part. There are a wide variety of appearance defects in tab welding, including scratches, breakage, and wrinkles in the tab itself, as well as various defects such as solder skips, over-welding, and poor welding status in the welding process. The acceptance requirements are high, and the size of the defect area needs to be considered, which cannot be solved by the existing visual inspection solutions.




   Defect types:


     Defects of the tab itself, such as scratches, breakage, and wrinkles, as well as solder skips, over-welding, and poor welding status in the welding process.





             Online full inspection, cost savings of 60%        70% increase in production efficiency